Atomic layer deposition of Ti-doped ZnO films with enhanced electron mobility

Do Joong Lee, Ki Ju Kim, Soo Hyun Kim, Jang Yeon Kwon, Jimmy Xu, Ki Bum Kim

Research output: Contribution to journalArticlepeer-review

36 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Atomic layer deposition of Ti-doped ZnO films with enhanced electron mobility'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemistry