Translated title of the contribution | Investigation of mechanical properties and microstructure of cement paste with glass beads using crack phase field model and lineal-path function |
---|---|
Original language | Polish |
Pages (from-to) | 239-250 |
Number of pages | 12 |
Journal | Cement, Wapno, Beton |
Volume | 2018 |
Issue number | 3 |
Publication status | Published - 2018 |
Bibliographical note
Funding Information:Authors would like to thank Dr. Xiaoxuan Zhang and Prof. Christian Linder for guidance and discussions on the crack phase field model. This research was supported by the National Research Foundation Grant, funded by the Korean Government and was supported by the German Federal Ministry of Education and Research for KONNECT Joint Call project (NRF-2015K1A3A1A59073929/BMBF Project number: 01DR16007). This work was also supported by the Korea Institute of Energy Technology Evaluation and Planning (KETEP) and the Ministry of Trade, Industry & Energy (MOTIE) of the Republic of Korea (No. 20174030201480). Parallel computation in this work was supported by the PLSI supercomputing resources of the Korea Institute of Science and Technology Information and the resources of the UNIST Supercomputing Center. μ-CT images were obtained from the synchrotron operated by the Pohang Accelerator Laboratory (PAL) in Korea.
All Science Journal Classification (ASJC) codes
- Building and Construction
- Materials Science(all)