Effect oxygen exposure on the quality of atomic layer deposition of ruthenium from bis(cyclopentadienyl)ruthenium and oxygen

Sang Joon Park, Woo Hee Kim, W. J. Maeng, Y. S. Yang, C. G. Park, Hyungjun Kim, Kook Nyung Lee, Suk Won Jung, W. K. Seong