Investigation on the atomic layer deposition of the Se doped Sb–Te phase change films using an alkyl-silyl precursor

Jin Hwan Jeong, Doo Jin Choi

Research output: Contribution to journalArticlepeer-review

5 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Investigation on the atomic layer deposition of the Se doped Sb–Te phase change films using an alkyl-silyl precursor'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy

Chemical Compounds